Freeze–Thaw Damage Mitigation in Steel Fiber Concrete Using GO–MWCNT Hybrid Nano-Modification

M. Hosseininasr, S.Mohammad Mirhosseini, Ali Hassani Joshaghani, Ehsanollah Zeighami, Behnoosh Khataei
November 20, 2026
Published Date

Research Abstract & Technology Focus

Freeze-thaw (F-T) cycling remains a critical durability challenge for concrete in cold climates, as internal ice formation generates hydraulic pressure, causing microcracking and strength degradation. This study investigates the synergistic effects of graphene oxide (GO) and multi-walled carbon nanotubes (MWCNTs) on the mechanical properties and freeze-thaw resistance of steel fiber-reinforced concrete (SFRC). Mixtures containing 0.02, 0.04, and 0.06 wt% GO (by cement mass) with a fixed 0.15 wt% MWCNT content were subjected to 300 freeze-thaw cycles. Durability performance was evaluated using residual mechanical properties and mass loss. Compressive, splitting tensile, and flexural strengths, together with mass loss, were measured before and after cycling (n = 3 per condition). SEM/ImageJ porosity, XRD, life-cycle assessment (LCA), and life-cycle costing (LCC) were performed. Among the investigated mixtures, the hybrid containing 0.04 wt% GO and 0.15 wt% MWCNTs achieved the best overall performance, increasing 28-day compressive strength by 21% (29.0 ± 0.8 to 35.0 ± 0.8 MPa). After 300 F-T cycles, compressive strength loss decreased from 40% to 22% at 28 days and from 21% to 12% at 90 days. Splitting tensile and flexural strengths increased by 34% and 56%, respectively, while mass loss decreased by 39%. Microstructural analyses indicated reduced porosity, lower portlandite content, and enhanced C-S-H formation. LCA showed approximately 18% lower CO₂-eq emissions, while LCC demonstrated reduced maintenance requirements over the service life, lowering total life-cycle cost by about 11.6%. The reported durability results are based on endpoint measurements, as the relative dynamic modulus was not monitored during freeze-thaw cycling.
Read Full Literature

Frequently Asked Questions (FAQ)

Curated market intelligence mapped to this research.

What is the core focus of the research titled 'Freeze–Thaw Damage Mitigation in Steel Fiber Concrete Using GO–MWCNT Hybrid Nano-Modification'?

This literature focuses on: Freeze-thaw (F-T) cycling remains a critical durability challenge for concrete in cold climates, as internal ice formation generates hydraulic pressure, causing microcracking and strength degradation. This study investigates the synergistic effect...